| 规格级别 | 其它 薄膜 其它 | 外观颜色 | |
| 该料用途 | |||
| 备注说明 | 低密度、高光滑性、光学性能、良好的剥离性、 中等抗结块性 | ||
| 性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | |
| 物理性能 | 密度 | ASTM D1505 | 0.924 | g/cm³ | |
| 熔流率 | 190°C/2.16 kg | ASTM D1238 | 5.0 | g/10 min | |
| 硬度计硬度 | 支撐 D | ASTM D2240 | 52 | ||
| 机械性能 | 抗张强度 | 屈服 | ASTM D638 | 10.8 | MPa | 
| 断裂 | ASTM D638 | 13.7 | MPa | ||
| 伸长率 | 断裂 | ASTM D638 | 600 | % | |
| 弯曲模量 | ASTM D790 | 177 | MPa | ||
| 摩擦系数 | 吹塑薄膜 | ASTM D1894 | 0.12 | ||
| 薄膜厚度 | 经测试 | 30 | µm | ||
| 可供应的薄膜厚度 | 0.6-2.4 | mil | |||
| 割线模量 | 1% 正割, MD: 38 µm, 吹塑薄膜 | ASTM D882 | 186 | MPa | |
| 1% 正割, TD: 38 µm, 吹塑薄膜 | ASTM D882 | 216 | MPa | ||
| 抗张强度 | MD: 屈服, 38 µm, 吹塑薄膜 | ASTM D882 | 10.8 | MPa | |
| TD: 屈服, 38 µm, 吹塑薄膜 | ASTM D882 | 11.8 | MPa | ||
| MD: 断裂, 38 µm, 吹塑薄膜 | ASTM D882 | 16.7 | MPa | ||
| TD: 断裂, 38 µm, 吹塑薄膜 | ASTM D882 | 14.7 | MPa | ||
| 伸长率 | MD: 断裂, 38 µm, 吹塑薄膜 | ASTM D882 | 270 | % | |
| TD: 断裂, 38 µm, 吹塑薄膜 | ASTM D882 | 500 | % | ||
| 落锤冲击 | 38 µm, 吹塑薄膜 | ASTM D1709 | 70 | g | |
| 埃尔曼多夫抗撕强度 | MD: 38 µm, 吹塑薄膜 | ASTM D1922 | 240 | g | |
| TD: 38 µm, 吹塑薄膜 | ASTM D1922 | 180 | g | ||
| 热性能 | 脆化温度 | ASTM D746 | -70.0 | °C | |
| 维卡软化温度 | ASTM D1525 | 92.0 | °C | ||
| 熔融温度 | ASTM D1525 | 112 | °C | ||