| 规格级别 | 其它 薄膜 吹塑 | 外观颜色 | |
| 该料用途 | |||
| 备注说明 | 低密度、高拉伸强度、抗穿孔性、抗氧化性、 良好的剥离性、良好的热封性 | ||
| 性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | |
| 物理性能 | 密度 | ASTM D1505 | 0.920 | g/cm³ | |
| 熔流率 | 190°C/2.16 kg | ASTM D1238 | 1.0 | g/10 min | |
| 薄膜 | 薄膜厚度 | 经测试 | 38 | µm | |
| 割线模量 | 1% 正割, MD: 38 µm, 吹塑薄膜 | ASTM D882 | 142 | MPa | |
| 1% 正割, TD: 38 µm, 吹塑薄膜 | ASTM D882 | 157 | MPa | ||
| 抗张强度 | MD: 屈服, 38 µm, 吹塑薄膜 | ASTM D882 | 9.81 | MPa | |
| TD: 屈服, 38 µm, 吹塑薄膜 | ASTM D882 | 10.8 | MPa | ||
| MD: 断裂, 38 µm, 吹塑薄膜 | ASTM D882 | 40.2 | MPa | ||
| TD: 断裂, 38 µm, 吹塑薄膜 | ASTM D882 | 31.4 | MPa | ||
| 伸长率 | MD: 断裂, 38 µm, 吹塑薄膜 | ASTM D882 | 620 | % | |
| TD: 断裂, 38 µm, 吹塑薄膜 | ASTM D882 | 840 | % | ||
| 落锤冲击 | 38 µm, 吹塑薄膜 | ASTM D1709 | 150 | g | |
| 埃尔曼多夫抗撕强度 | MD: 38 µm, 吹塑薄膜 | ASTM D1922 | 220 | g | |
| TD: 38 µm, 吹塑薄膜 | ASTM D1922 | 560 | g | ||
| 热性能 | 脆化温度 | ASTM D746 | -70.0 | °C | |
| 维卡软化温度 | ASTM D1525 | 93.0 | °C | ||
| 熔融温度 | ASTM D1525 | 122 | °C | ||