规格级别 | 外观颜色 | ||
该料用途 | |||
备注说明 |
性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | |
物理性能 | 密度 | ASTMD1505 | 0.920 | g/cm³ | |
物理性能 | 熔流率(熔体流动速率)(190°C/2.16kg) | ASTMD1238 | 2.0 | g/10min | |
薄膜 | 薄膜厚度-经测试 | 38 | µm | ||
薄膜 | SecantModulus-1%Secant,MD(38µm) | ASTMD882 | 175 | MPa | |
薄膜 | SecantModulus-1%Secant,TD(38µm) | ASTMD882 | 205 | MPa | |
薄膜 | TensileStrength-MD(Yield,38µm) | ASTMD882 | 10.0 | MPa | |
薄膜 | TensileStrength-TD(Yield,38µm) | ASTMD882 | 10.0 | MPa | |
薄膜 | TensileStrength-MD(Break,38µm) | ASTMD882 | 25.0 | MPa | |
薄膜 | TensileStrength-TD(Break,38µm) | ASTMD882 | 19.0 | MPa | |
薄膜 | TensileElongation-MD(Break,38µm) | ASTMD882 | 300 | % | |
薄膜 | TensileElongation-TD(Break,38µm) | ASTMD882 | 600 | % | |
薄膜 | 落锤冲击(38µm) | ASTMD1709A | 150 | g | |
薄膜 | ElmendorfTearStrength-MD(38µm) | ASTMD1922 | 180 | g | |
薄膜 | ElmendorfTearStrength-TD(38µm) | ASTMD1922 | 130 | g | |
热性能 | 熔融峰值温度 | ASTMD3418 | 111 | °C | |
光学性能 | Gloss(45°,38.0µm) | ASTMD2457 | 50 | ||
光学性能 | Haze(38.0µm) | ASTMD1003 | 11 | % |