规格级别 | 外观颜色 | ||
该料用途 | |||
备注说明 |
性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | |
物理性能 | 密度 | ASTMD1505 | 0.921 | g/cm³ | |
物理性能 | 熔流率(熔体流动速率)(190°C/2.16kg) | ASTMD1238 | 1.8 | g/10min | |
薄膜 | 薄膜厚度-经测试 | 32 | µm | ||
薄膜 | SecantModulus-1%Secant,MD(32µm) | ASTMD882 | 179 | MPa | |
薄膜 | SecantModulus-1%Secant,TD(32µm) | ASTMD882 | 207 | MPa | |
薄膜 | TensileStrength-MD(Yield,32µm) | ASTMD882 | 11.0 | MPa | |
薄膜 | TensileStrength-MD(Break,32µm) | ASTMD882 | 27.6 | MPa | |
薄膜 | TensileStrength-TD(Break,32µm) | ASTMD882 | 23.4 | MPa | |
薄膜 | TensileElongation-MD(Break,32µm) | ASTMD882 | 300 | % | |
薄膜 | TensileElongation-TD(Break,32µm) | ASTMD882 | 500 | % | |
薄膜 | 落锤冲击(32µm) | ASTMD1709 | 90 | g | |
薄膜 | 埃尔曼多夫抗撕强度-MD(32µm) | ASTMD1922 | 360 | g | |
薄膜 | ElmendorfTearStrength-TD(32µm) | ASTMD1922 | 200 | g | |
热性能 | 维卡软化温度 | ASTMD1525 | 100 | °C |